SEM (scanning electron microscope) images of the fracture surfaces of the samples were obtained on Jeol JSM 5800 with a voltage
of 10 kV and the pressure of 10−5 Pa. Samples were previously
cracked in liquid nitrogen and coated with gold alloy to improve
conductivity and prevent charging